| POLYURETHANE R.I.M. MATERIALS |
POLYURETHANE |
DESCRIPTION |
POT-LIFE MINUTES
@
25 deg C
|
PACK SIZE |
VISCOSITY
mPa.s
@
25 deg C
|
HARDNESS
AFTER 48 Hrs |
APPLICATION |
| PU 3827 A + B |
Black, high
elongation & impact strength, simulates polypropylene. Good mould
penetration and fast de-mould. |
50-55 sec |
9 kg 45 kg |
600-800 |
75-80 D |
Low to medium
pressure RIM where high strength is required. |
| PU 3828 A + B |
Black, very
high heat resistance (180°c). Low viscosity and rapid de-mould |
45-50 sec |
9kg |
600 |
82 D |
Low to medium
pressure RIM where high thermal properties are required. Under bonnet
|
| PU 3829 A + B |
Black, longer
potlife and high modulus. HDT 124°C. |
80-90 sec |
9 kg 45 kg |
500 |
82 D |
Low to medium
pressure RIM where high strength is required |